(Created page with "<gallery caption="Recipe no. 10: C06445_02 coil_2500W, platen:300W, He/C4F8= 17.5, C4F8/H2=1, Pressure:8.8mTorr, C4F8:25.6sccm, He:448.7sccm, H2:25.6sccm, 3:56 min " perrow="8...") |
No edit summary |
||
Line 1: | Line 1: | ||
==SiO2 Etch== | |||
I am in the process of doing some development of a SiO2 etch. So far I have found this fairly good recipe. For now it is the standard SiO2 etch recipes but I might change the "Standard recipe" a a later time if I find a better one. You are welcome to contact me see more result. I will add them to Labadviser at a later time. | |||
/Berit Herstrøm bghe@dtu.dk (Nanolab) | |||
<gallery caption="Recipe no. 10: C06445_02 coil_2500W, platen:300W, He/C4F8= 17.5, C4F8/H2=1, Pressure:8.8mTorr, C4F8:25.6sccm, He:448.7sccm, H2:25.6sccm, 3:56 min " perrow="8"> | <gallery caption="Recipe no. 10: C06445_02 coil_2500W, platen:300W, He/C4F8= 17.5, C4F8/H2=1, Pressure:8.8mTorr, C4F8:25.6sccm, He:448.7sccm, H2:25.6sccm, 3:56 min " perrow="8"> | ||
Revision as of 09:33, 5 February 2021
SiO2 Etch
I am in the process of doing some development of a SiO2 etch. So far I have found this fairly good recipe. For now it is the standard SiO2 etch recipes but I might change the "Standard recipe" a a later time if I find a better one. You are welcome to contact me see more result. I will add them to Labadviser at a later time. /Berit Herstrøm bghe@dtu.dk (Nanolab)
- Recipe no. 10: C06445_02 coil_2500W, platen:300W, He/C4F8= 17.5, C4F8/H2=1, Pressure:8.8mTorr, C4F8:25.6sccm, He:448.7sccm, H2:25.6sccm, 3:56 min