Nickel can be deposited by e-beam evaporation or electroplating. In the chart below you can compare the different deposition equipment. | Nickel can be deposited by e-beam evaporation, sputtering or electroplating. In the chart below you can compare the different deposition equipment. | ||
*[[/Electroplating of nickel|Electroplating of nickel]] | *[[/Electroplating of nickel|Electroplating of nickel]] | ||
Line 49: | Line 49: | ||
|10 Å to 5000 Å ** | |10 Å to 5000 Å ** | ||
|10 Å to 5000 Å ** | |10 Å to 5000 Å ** | ||
|~20 µm to ~1000 µm | |~ 20 µm to ~ 1000 µm | ||
|- | |- | ||
|-style="background:LightGrey; color:black" | |-style="background:LightGrey; color:black" | ||
! Deposition rate | ! Deposition rate | ||
| | |2-10 Å/s | ||
| | |10-15 Å/s | ||
|1 | |1-10 Å/s | ||
|Depends on process parameters | |Depends on process parameters, about 1 Å/s | ||
|Depends on process parameters | |Depends on process parameters | ||
| | |~ 10-250 Å/s | ||
|-style="background:WhiteSmoke; color:black" | |-style="background:WhiteSmoke; color:black" | ||
Line 127: | Line 127: | ||
* Metals | * Metals | ||
| | | | ||
*Almost any that do not outgas | *Almost any that do not outgas. Check the cross-contamination sheets in Labmanager. | ||
| | | | ||
Base materials:<br> | Base materials:<br> | ||
Line 144: | Line 144: | ||
|-style="background:WhiteSmoke; color:black" | |-style="background:WhiteSmoke; color:black" | ||
! Comment | ! Comment | ||
| | | | ||
| | | | ||
*[[/Stress Wordentec Ni films|Stress in Wordentec Ni films: study here]]. | *[[/Stress Wordentec Ni films|Stress in Wordentec Ni films: study here]]. | ||
| | | | ||
| | | | ||
*May use high-strength magnet for deposition. | *May use high-strength magnet for deposition. | ||
| | | | ||
*May use high-strength magnet for deposition | *May use high-strength magnet for deposition | ||
* | | | ||
*Sample must be compatible with plating bath (pH = 3,65 and T = 52°C). Seed metal necessary. | |||
|- | |- | ||
|} | |} | ||
'''*''' ''To deposit | '''*''' ''To deposit a cumulative thickness above 600 nm permission is required from metal@nanolab.dtu.dk to ensure enough material is present in the machine'' | ||
'''**''' ''To deposit | '''**''' ''To deposit a cumulative thickness above 200 nm permission is required from metal@nanolab.dtu.dk to ensure enough material is present in the machine'' |
Revision as of 10:44, 21 April 2020
Feedback to this page: click here
Nickel deposition
Nickel can be deposited by e-beam evaporation, sputtering or electroplating. In the chart below you can compare the different deposition equipment.
E-beam evaporation (Temescal) | E-beam evaporation (Wordentec) | E-beam evaporation (Physimeca) | Sputter deposition (Lesker) | Sputter deposition (Cluster-based sputter system) | Electroplating (Electroplating-Ni) | |
---|---|---|---|---|---|---|
General description | E-beam deposition of Nickel | E-beam deposition of Nickel | E-beam deposition of Nickel | Sputter deposition of Nickel | Sputter deposition of Nickel | Electroplating of Nickel |
Pre-clean | Ar ion bombardment | RF Ar clean | RF Ar clean | RF Ar clean | None | |
Layer thickness | 10 Å to 1 µm * | 10 Å to 1 µm * | 10 Å to 2000 Å | 10 Å to 5000 Å ** | 10 Å to 5000 Å ** | ~ 20 µm to ~ 1000 µm |
Deposition rate | 2-10 Å/s | 10-15 Å/s | 1-10 Å/s | Depends on process parameters, about 1 Å/s | Depends on process parameters | ~ 10-250 Å/s |
Batch size |
|
|
|
|
|
|
Allowed materials |
|
|
|
|
|
Base materials:
Seed metals:
|
Comment |
|
|
|
* To deposit a cumulative thickness above 600 nm permission is required from metal@nanolab.dtu.dk to ensure enough material is present in the machine
** To deposit a cumulative thickness above 200 nm permission is required from metal@nanolab.dtu.dk to ensure enough material is present in the machine