Specific Process Knowledge/Thin film deposition/Deposition of Nickel: Difference between revisions
→Nickel deposition: edited limits for permission |
|||
Line 161: | Line 161: | ||
'''*''' ''To deposit layers thicker than 600 nm permission is required from metal@nanolab.dtu.dk to ensure enough material is present in the machine'' | '''*''' ''To deposit layers thicker than 600 nm permission is required from metal@nanolab.dtu.dk to ensure enough material is present in the machine'' | ||
'''**''' ''To deposit layers thicker than 200 nm permission is required from metal@nanolab.dtu.dk to ensure enough material is present in the machine'' | '''**''' ''To deposit layers thicker than 200 nm permission is required from metal@nanolab.dtu.dk to ensure enough material is present in the machine'' |
Revision as of 10:40, 21 April 2020
Feedback to this page: click here
Nickel deposition
Nickel can be deposited by e-beam evaporation or electroplating. In the chart below you can compare the different deposition equipment.
E-beam evaporation (Temescal) | E-beam evaporation (Wordentec) | E-beam evaporation (Physimeca) | Sputter deposition (Lesker) | Sputter deposition (Cluster-based sputter system) | Electroplating (Electroplating-Ni) | |
---|---|---|---|---|---|---|
General description | E-beam deposition of Nickel | E-beam deposition of Nickel | E-beam deposition of Nickel | Sputter deposition of Nickel | Sputter deposition of Nickel | Electroplating of Nickel |
Pre-clean | Ar ion bombardment | RF Ar clean | RF Ar clean | RF Ar clean | None | |
Layer thickness | 10 Å to 1 µm * | 10 Å to 1 µm * | 10 Å to 2000 Å | 10 Å to 5000 Å ** | 10 Å to 5000 Å ** | ~20 µm to ~1000 µm |
Deposition rate | 2Å/s to 10Å/s | 10Å/s to 15Å/s | 1 to 10Å/s | Depends on process parameters. About 1 Å/s | Depends on process parameters. | About 10 Å/s to 250 Å/s |
Batch size |
|
|
|
|
|
|
Allowed materials |
|
|
|
|
|
Base materials:
Seed metals:
|
Comment | Thicknesses above 2000 Å requires special permission |
|
|
|
Sample must be compatible with plating bath (pH = 3,65 and T = 52°C). Seed metal necessary. |
* To deposit layers thicker than 600 nm permission is required from metal@nanolab.dtu.dk to ensure enough material is present in the machine
** To deposit layers thicker than 200 nm permission is required from metal@nanolab.dtu.dk to ensure enough material is present in the machine