Specific Process Knowledge/Thin film deposition/Deposition of Titanium Nitride: Difference between revisions
Line 6: | Line 6: | ||
== Deposition of Titanium Nitride == | == Deposition of Titanium Nitride == | ||
Thin films of Titanium Nitride (TiN) can be deposited by either [[Specific Process Knowledge/Thin film deposition/ALD2 (PEALD)|ALD]] or [[Specific Process Knowledge/Thin film deposition/Lesker|sputtering]] methods. | Thin films of Titanium Nitride (TiN) can be deposited by either [[Specific Process Knowledge/Thin film deposition/ALD2 (PEALD)|ALD]] or [[Specific Process Knowledge/Thin film deposition/Lesker|reactive sputtering]] methods. | ||
Information about the ALD process can be found [[Specific Process Knowledge/Thin film deposition/ALD2 (PEALD)/TiN deposition using ALD2|here]]. | *Information about the ALD process can be found [[Specific Process Knowledge/Thin film deposition/ALD2 (PEALD)/TiN deposition using ALD2|here]]. | ||
Information about the sputtering method can be found [[Specific Process Knowledge/Thin film deposition/Deposition of Titanium Nitride/Deposition of Titanium Nitride using Lesker sputter tool|here]]. | If sputtering method is used the target is Ti and nitrogen (N<sub>2</sub>) is added as reactive gas to the chamber resulting the formation of Titanium Nitride on the sample. | ||
*Information about the sputtering method can be found [[Specific Process Knowledge/Thin film deposition/Deposition of Titanium Nitride/Deposition of Titanium Nitride using Lesker sputter tool|here]]. | |||
==Comparison between sputtering and ALD methods for deposition of Titanium Nitride.== | ==Comparison between sputtering and ALD methods for deposition of Titanium Nitride.== |
Revision as of 15:46, 6 April 2020
Feedback to this page: click here
Deposition of Titanium Nitride
Thin films of Titanium Nitride (TiN) can be deposited by either ALD or reactive sputtering methods.
- Information about the ALD process can be found here.
If sputtering method is used the target is Ti and nitrogen (N2) is added as reactive gas to the chamber resulting the formation of Titanium Nitride on the sample.
- Information about the sputtering method can be found here.
Comparison between sputtering and ALD methods for deposition of Titanium Nitride.
ALD2 | Sputter System Lesker | |
---|---|---|
Generel description |
|
|
Stoichiometry |
|
|
Film Thickness |
|
|
Deposition rate |
|
|
Step coverage |
|
|
Process Temperature |
|
|
Substrate size |
|
|
Allowed materials |
|
|