Deposition of Germanium
Germanium can be deposited by thermal evaporation and e-beam evaporation.
Thermal deposition
Ge deposition equipment comparison
Thermal evaporation (Wordentec) | E-beam evaporation (Physimeca) | E-beam evaporation (Temescal) | |
---|---|---|---|
General description | Thermal deposition of Ge | E-beam deposition of Ge | E-beam deposition of Ge |
Pre-clean | RF Ar clean | - | Ar ion beam clean |
Layer thickness | 10Å to about 2000Å (in total distributed on all loaded wafers) | 10Å to about 3000Å | 10Å to about 1000 nm |
Deposition rate | From 0.4 Å/s up to about ~2Å/s | 5 Å/s | From 1 Å/s up to 5 Å/s |
Batch size |
Many small pieces |
|
|
Allowed substrates |
|
|
|
Allowed materials |
|
|
|
Comment | Recommended for unexposed e-beam resist |