Specific Process Knowledge/Characterization/Probe station: Difference between revisions

From LabAdviser
Jump to navigation Jump to search
No edit summary
Line 2: Line 2:
[[Image:probe2.jpg|thumb|300x300px|Probe station. Positioned in serviceroom CX1]]
[[Image:probe2.jpg|thumb|300x300px|Probe station. Positioned in serviceroom CX1]]


'''Feedback to this page''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Characterization/Probe_Station click here]'''
'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Characterization/Probe_station click here]'''


The Probe station is a - EPS150Triax - Cascade. The purpose is to measure I/V measurement, ohmic measurements etc. It has 4 individually adjustable triax connected probes, but can be fitted with additional coax connected probes. The stage can be moved in x and y to step and repeat a measurement over a large number of chips.
The Probe station is a - EPS150Triax - Cascade. The purpose is to measure I/V measurement, ohmic measurements etc. It has 4 individually adjustable triax connected probes, but can be fitted with additional coax connected probes. The stage can be moved in x and y to step and repeat a measurement over a large number of chips.

Revision as of 08:45, 18 March 2020

Probe station

Probe station. Positioned in serviceroom CX1

Feedback to this page: click here

The Probe station is a - EPS150Triax - Cascade. The purpose is to measure I/V measurement, ohmic measurements etc. It has 4 individually adjustable triax connected probes, but can be fitted with additional coax connected probes. The stage can be moved in x and y to step and repeat a measurement over a large number of chips.

Samples can be inspected by either a microscope and/or a camera.

Two Keithley 2450 source meters are connected to the probe station by triax cables. An additional Keithley 2410 source meter and a Keithley 2000 multi meter is connected by coax cables. All Keithleys can also be connected with banana wires.

Equipment performance and process related parameters

Purpose

Electrical measurements

  • I/V
  • Resistance
  • Data collection by PC possible

Performance

Pad size

  • 100x100µm or more

Substrates

Batch size

  • One sample
Substrate materials allowed
  • No restrictions