Specific Process Knowledge/Etch/DRIE-Pegasus/showerheadchange/ProcessD/PrD-3: Difference between revisions
No edit summary |
No edit summary |
||
Line 23: | Line 23: | ||
| Pegasus/jmli | | Pegasus/jmli | ||
| 10 minute TDESC clean | | 10 minute TDESC clean | ||
| | | nanolab/jml/showerhead/prD/PrD-3, 150 cyc or 8:48 mins | ||
| S004781 | | S004781 | ||
! New showerhead | ! New showerhead |
Revision as of 22:27, 25 November 2019
Date | Substrate Information | Process Information | SEM Images | ||||||
---|---|---|---|---|---|---|---|---|---|
Wafer info | Mask | Material/ Exposed area | Tool / Operator | Conditioning | Recipe | Wafer ID | Comments | ||
8/1-2015 | 4" Wafer with travkaXX mask | AZ standard | Si / XX % | Pegasus/jmli | 10 minute TDESC clean | nanolab/jml/showerhead/prD/PrD-3, 150 cyc or 8:48 mins | S004781 | New showerhead |