Gold can be deposited by e-beam evaporation. In the chart below you can compare the different deposition equipment.
E-beam evaporation (Alcatel) | E-beam evaporation (Leybold) | E-beam evaporation (Wordentec) | Sputter (Lesker) | |
---|---|---|---|---|
Batch size |
|
|
|
|
Pre-clean | RF Ar clean | Ar ion bombartment | RF Ar clean | RF Ar clean |
Layer thickness | 10Å to 1µm | 10Å to 1500 Å | 10Å to 1 µm | 10Å to |
Deposition rate | 2Å/s to 15Å/s | 1Å/s to 5Å/s | 1Å/s to 15Å/s |
Studies of Au deposition processes
Roughness of Au layers - Roughness of Au layers deposited with different equipment and settings