Deposition of aluminium oxide
Aluminium oxide (Alumina, Al2O3 ) can be deposited by use of ALD (atomic layer deposition) or by a sputter technique in the Lesker Sputter System. During the sputter deposition oxygen is added to the chamber resulting in aluminium oxide on the sample
Comparison of the methods for deposition of Alumium Oxide
Sputter System Lesker | ALD Picosun 200 | |
---|---|---|
Generel description |
|
|
Stoichiometry |
|
|
Film Thickness |
|
|
Deposition rate |
|
|
Step coverage |
|
|
Process Temperature |
|
|
More info on Al2O3 | ||
Substrate size |
|
|
Allowed materials |
|
|