'''Feedback to this page''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php?title=Specific_Process_Knowledge/Thin_film_deposition/Deposition_of_AZO&action=edit click here]''' | '''Feedback to this page''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php?title=Specific_Process_Knowledge/Thin_film_deposition/Deposition_of_AZO&action=edit click here]''' | ||
Revision as of 11:10, 7 April 2017
Feedback to this page: click here
AZO can be deposited by Sputtering process and atomic layer deposition (ALD). In the chart below you can compare the different deposition equipment.
Sputtering deposition (Lesker) | Atomic layer deposition (ALD Picosun R200) | |
---|---|---|
General description | Sputter deposition of AZO | Atomic layer deposition of AZO |
Pre-clean | RF Ar clean | |
Layer thickness | 10Å to 5000Å* | 0 to 1000 Å |
Deposition rate | Depending on process parameters. | Depending on temperature |
Batch size |
|
|
Allowed materials |
|
|
Comment |
|
* For thicknesses above 200 nm permission is required.