Specific Process Knowledge/Thin film deposition/Deposition of AZO: Difference between revisions
Created page with "'''Feedback to this page''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php?title=Specific_Process_Knowled..." |
|||
Line 11: | Line 11: | ||
! | ! | ||
! | ! Sputtering deposition ([[Specific Process Knowledge/Thin film deposition/Lesker|Lesker]]) | ||
! Atomic layer deposition ([[Specific_Process_Knowledge/Thin_film_deposition/ALD_Picosun_R200|ALD Picosun R200]]) | ! Atomic layer deposition ([[Specific_Process_Knowledge/Thin_film_deposition/ALD_Picosun_R200|ALD Picosun R200]]) | ||
|- | |- |
Revision as of 12:32, 30 January 2017
Feedback to this page: click here
THIS PAGE IS UNDER CONSTRUCTION
AZO can be deposited by Sputtering process and atomic layer deposition (ALD). In the chart below you can compare the different deposition equipment.
Sputtering deposition (Lesker) | Atomic layer deposition (ALD Picosun R200) | |
---|---|---|
General description | Sputter deposition of AZO | Atomic layer deposition of AZO |
Pre-clean | RF Ar clean | RF Ar clean |
Layer thickness | 10Å to 1µm* | 10Å to |
Deposition rate | 2Å/s to 15Å/s | ~0.3Å/s |
Batch size |
|
|
Allowed materials |
|
|
Comment |
* For thicknesses above 200 nm permission is required.