Tungsten (W) can be deposited by e-beam evaporation. In the chart below you can compare the different deposition equipment.


E-beam evaporation (Alcatel)
General description E-beam evaporation of W
Pre-clean RF Ar clean
Layer thickness 10Å to 5000Å*
Deposition rate 2Å/s to 15Å/s
Batch size
  • Up to 1x4" wafers
  • small pieces
Allowed materials
  • Silicon
  • Silicon oxide
  • Silicon (oxy)nitride
  • Photoresist
  • PMMA
  • Mylar
  • SU-8
  • Metals
Comments

* For thicknesses above 200 nm permission is required