Specific Process Knowledge/Etch/Etching of Silicon Oxide/SiO2 etch using AOE/Standard recipe with resist mask/Striation: Difference between revisions
< Specific Process Knowledge | Etch | Etching of Silicon Oxide | SiO2 etch using AOE | Standard recipe with resist mask
Jump to navigation
Jump to search
Line 7: | Line 7: | ||
# deposition on the sidewalls as the etch proceeds, coursing masking effects | # deposition on the sidewalls as the etch proceeds, coursing masking effects | ||
# | #* This can come from flour-carbon polymers from the plasma (some this this layer protects from striation) | ||
# | #* Re-deposition of sputtered SiO2 | ||
# damage of the resist mask coursed by plasma heating and/or interaction with the resist. | # damage of the resist mask coursed by plasma heating and/or interaction with the resist. | ||
# | #* Resist edge get rough during etching due to plasma heating (out-gassing while the surface get UV hardened. This make the resist crumple). The edge can maybe also get roughened due to sputtering. This pattern change at the edge gets transferred to the oxide profile during the etch. | ||
Revision as of 08:59, 20 April 2016
Feedback to this page: click here
Striation: Side wall roughness
When etching silicon oxide rough sidewalls are most often seem. This effect is called striation, because it creates stripes along the etched profile. The literature gives several coarses for this. The two main courses seems to be:
- deposition on the sidewalls as the etch proceeds, coursing masking effects
- This can come from flour-carbon polymers from the plasma (some this this layer protects from striation)
- Re-deposition of sputtered SiO2
- damage of the resist mask coursed by plasma heating and/or interaction with the resist.
- Resist edge get rough during etching due to plasma heating (out-gassing while the surface get UV hardened. This make the resist crumple). The edge can maybe also get roughened due to sputtering. This pattern change at the edge gets transferred to the oxide profile during the etch.
Sidewall roughness and resist surface after etch viewed with SEM
- Striation with different resists used
Roughness of the resist after etch measured with the AFM