! rowspan="2" width="100"| Continuous black silicon recipe on blank wafer | ! rowspan="2" width="100"| Continuous black silicon recipe on blank wafer | ||
| rowspan="2" width="100"| 15 mins, -10 degrees, 32 mtorr, 60 sccm SF<sub>6</sub>, 55 sccm O<sub>2</sub>, 70 W platen | |||
| S004592 | | S004592 | ||
| Wafer centre | | Wafer centre |