Line 13: | Line 13: | ||
! SEM images | ! SEM images | ||
|- | |- | ||
! rowspan="2"| | ! rowspan="2"| 15 minutes of black silicon recipe on blank wafer | ||
| S004592 | | S004592 | ||
| Wafer centre | | Wafer centre |