Specific Process Knowledge/Etch/Etching of Chromium: Difference between revisions
Jump to navigation
Jump to search
Line 57: | Line 57: | ||
|Allowed materials | |Allowed materials | ||
| | | | ||
No restrictions | No restrictions. | ||
Make a note on the beaker of which materials have been processed. | Make a note on the beaker of which materials have been processed. | ||
| | | | ||
No restrictions | No restrictions. | ||
Make a note on the beaker of which materials have been processed. | Make a note on the beaker of which materials have been processed. | ||
|- | |- | ||
|} | |} |
Revision as of 10:24, 31 January 2008
Etching of Chromium
Etching of chromium is done wet at Danchip making your own set up in a beaker in a fumehood - preferably in cleanroom 2 or 4. We have two solution for this:
- HNO:HO:cerisulphate - 90ml:1200ml:15g - standard at Danchip
- Commercial chromium etch
Etch rate are depending on the level of oxidation of the metal.
Chromium etch 1 | Chromium etch 2 | |
---|---|---|
General description |
Etch of chromium |
Etch of chronium |
Chemical solution | HNO:HO:cerisulphate - 90ml:1200ml:15g | Commercial chromium etch
CE 8002-A |
Process temperature | Room temperature | Room temperature |
Possible masking materials: |
Photoresist (1.5 µm AZ5214E) |
Photoresist (1.5 µm AZ5214E) |
Etch rate |
~40-100 nm/min |
~10-20 nm/min |
Batch size |
1-25 wafers at a time |
1-25 wafer at a time |
Size of substrate |
4" wafers |
4" wafers |
Allowed materials |
No restrictions. Make a note on the beaker of which materials have been processed. |
No restrictions. Make a note on the beaker of which materials have been processed. |