Specific Process Knowledge/Thin film deposition/Deposition of Nickel: Difference between revisions
Line 105: | Line 105: | ||
*Thicknesses above 2000 Å requires special permission | *Thicknesses above 2000 Å requires special permission | ||
|Only very thin layers (up to 100nm). | |Only very thin layers (up to 100nm). | ||
|Sample must be compatible with plating bath. Seed metal necessary. | |Sample must be compatible with plating bath. Seed metal necessary. Never use gold directly on silicon. | ||
|- | |- | ||
Revision as of 10:59, 7 March 2014
Feedback to this page: click here
Nickel deposition
Nickel can be deposited by e-beam evaporation or electroplating. In the chart below you can compare the different deposition equipment.
E-beam evaporation (Alcatel) | E-beam evaporation (Wordentec) | E-beam evaporation (PVD co-sputter/evaporation) | Electroplating (Electroplating-Ni) | |
---|---|---|---|---|
Batch size |
|
|
|
|
Pre-clean | RF Ar clean | RF Ar clean | RF Ar clean | None |
Layer thickness | 10Å to 5000 Å* | 10Å to 1 µm* | 10Å to 1000 Å | A few µm to 1400 µm |
Deposition rate | 2Å/s to 15Å/s | 10Å/s to 15Å/s | About 1Å/s | About 10 Å/s to 250 Å/s
|
Allowed materials |
|
|
|
|
Comment | Thicknesses above 2000 Å requires special permission |
|
Only very thin layers (up to 100nm). | Sample must be compatible with plating bath. Seed metal necessary. Never use gold directly on silicon. |
* To deposit layers thicker then 2000 Å permission is required (contact Thin film group)