Removal of native oxide is a part of the RCA cleaning procedure. See the RCA page for further details. The HF/BHF baths in the RCA bench bath must only be used during the RCA cleaning procedure. For removal of oxide of processed wafers that is not getting a full RCA clean the other HF/BHF baths can be used. Please see the oxide etch page for more details.