File:Si2p.JPG
Si2p.JPG (730 × 572 pixels, file size: 27 KB, MIME type: image/jpeg)
XPS spectrum, Si2p (HF treated, not treated)
File history
Click on a date/time to view the file as it appeared at that time.
Date/Time | Thumbnail | Dimensions | User | Comment | |
---|---|---|---|---|---|
current | 09:27, 24 October 2011 | 730 × 572 (27 KB) | Kn (talk | contribs) | XPS spectrum, Si2p (HF treated, not treated) |
You cannot overwrite this file.