File:WF 2B1 feb06 2011-150.jpg
Jump to navigation
Jump to search
![File:WF 2B1 feb06 2011-150.jpg](/images/thumb/9/96/WF_2B1_feb06_2011-150.jpg/800px-WF_2B1_feb06_2011-150.jpg?20110316075303)
Size of this preview: 800 × 600 pixels. Other resolution: 1,024 × 768 pixels.
Original file (1,024 × 768 pixels, file size: 52 KB, MIME type: image/jpeg)
The profiles of the 180 nm thick zep resist wafers. The wafers have been over-exposed in the E-beam to make sure that all structures are opened - therefore the 30, 60, 90, 120 and 150 nm lines are somewhat wider.
File history
Click on a date/time to view the file as it appeared at that time.
Date/Time | Thumbnail | Dimensions | User | Comment | |
---|---|---|---|---|---|
current | 09:53, 16 March 2011 | ![]() | 1,024 × 768 (52 KB) | Jml (talk | contribs) | The profiles of the 180 nm thick zep resist wafers. The wafers have been over-exposed in the E-beam to make sure that all structures are opened - therefore the 30, 60, 90, 120 and 150 nm lines are somewhat wider. |
You cannot overwrite this file.
File usage
The following page uses this file: