Process runs
Date Substrate Information Process Information SEM Images
Wafer info Mask Material/ Exposed area Tool / Operator Conditioning Recipe Wafer ID Comments
8/1-2015 4" Wafer with travkaXX mask AZ standard Si / XX % Pegasus/jmli 10 minute TDESC clean nanolab/jml/showerhead/prD/PrD-3, 150 cyc or 8:48 mins S004781 New showerhead

S004781-04.jpg S004781-05.jpg S004781-03.jpg S004781-02.jpg S004781-01.jpg