Process runs
Date Substrate Information Process Information SEM Images
Wafer info Mask Material/ Exposed area Tool / Operator Conditioning Recipe Wafer ID Comments
20/11-2014 4" Wafer with AZ resist Travka50 pattern Si / 50+ % Pegasus/jmli 10 minute TDESC clean nanolab/jml/showerhead/prD, 110 cycles or 8:04 minutes S004584 Old showerhead

S004584-1.jpg S004584-3.jpg

1/12-2014 1/4 6" Wafer with 210 nm oxide and 1800 nm polysilicon crystalbonded on carrier standard stepper mask (50 nm barc + 320 nm krf) Si / 50+ % Pegasus/jmli 10 minute TDESC clean + 45 sec barc etch nanolab/jml/showerhead/polySi etch DUV mask, 20 cycles or 3:02 minutes S004675 New showerhead