Unless otherwise stated, this page is written by DTU Nanolab internal
An acceptance test was done after the installation in November 2021 by Tempress. For wet oxidation at 1050 C and 30 minutes, the thickness variation over a wafer was 1.3%(wafer in wafer), over the boat was 0.35%(wafer to wafer) and ran to ran was 0.64%.