  • curprev 11:5311:53, 26 January 2009Yg talk contribs 188 bytes +188 New page: The furnace A4 phosphorus predep can be used to predeposit silicon wafers with phosphor. The silicon wafers are positioned in a quarts boat. Phosphor is predeposited in the silicon wafers.