Wavelength [nm] | Objective [mm] | Scanfield [mm2] | Telescope Magnification | Rayleigh- length [mm] | Theoretical min Spotdiameter (1/e2) [um] | Working distance [mm] |
TB 355 | 103 | 45 x 45 | 3X | 0,972 | 21 | 135 |
TB 355 | 103 | 45 x 45 | 6X | 0,25 | 10,5 | 135 |
TB 355 | 255 | 145 x 145 | 3X | 5,96 | 51,9 | 313 |
TB 355 | 255 | 145 x 145 | 6X | 1,49 | 26 | 313 |
TB 532 | 100 | 54 x 54 | 3X | 0,823 | 23 | 126 |
TB 532 | 100 | 54 x 54 | 4X | 0,46 | 18 | 126 |
TB 532 | 255 | 165 x 165 | 3X | 5,35 | 60,2 | 293 |
TB 532 | 255 | 165 x 165 | 4X | 3,01 | 45,2 | 293 |
TB 1064 | 100 | 54 x 54 | 3X | 0,76 | 32,2 | 126 |
TB 1064 | 100 | 54 x 54 | 6X | 0,29 | 19,8 | 126 |
TB 1064 | 255 | 165 x 165 | 3X | 4,97 | 82 | 292 |
TB 1064 | 255 | 165 x 165 | 6X | 1,87 | 50,4 | 292 |
IPG 1064 | 100 | 54 x54 | 1X | 0,61 | 29 | 126 |
IPG 1064 | 255 | 165 x 165 | 1X | 3,99 | 73,5 | 292 |