Specific Process Knowledge/Thin film deposition/Deposition of Silicon Nitride: Difference between revisions
Line 5: | Line 5: | ||
Deposition of silicon nitride can be done with either LPCVD (Low Pressure Chemical Vapor Deposition) or PECVD (Plasma Enhanced Chemical Vapor Deposition). Stochiometric nitride or silicon rich (low stress) LPCVD nitride is deposited on a batch of wafers in a LPCVD nitride furnace, and PECVD nitride (or oxynitride) is deposited on a few samples at a time in a PECVD system. LPCVD nitride has a good step coverage and a very good uniformity. Using PECVD it is possible to deposit a much lower temperature and a thicker layer of nitride on different types of samples, but the nitride does not cover sidewalls very well. | Deposition of silicon nitride can be done with either LPCVD (Low Pressure Chemical Vapor Deposition) or PECVD (Plasma Enhanced Chemical Vapor Deposition). Stochiometric nitride or silicon rich (low stress) LPCVD nitride is deposited on a batch of wafers in a LPCVD nitride furnace, and PECVD nitride (or oxynitride) is deposited on a few samples at a time in a PECVD system. LPCVD nitride has a good step coverage and a very good uniformity. Using PECVD it is possible to deposit a much lower temperature and a thicker layer of nitride on different types of samples, but the nitride does not cover sidewalls very well. | ||
It is also possible to deposit silicon nitride using the Lesker sputter system | It is also possible to deposit silicon nitride using the Lesker sputter system. | ||
*[[Specific Process Knowledge/Thin film deposition/Furnace LPCVD Nitride/Deposition of stoichiometric nitride using the 4" LPCVD nitride furnace|Deposition of stoichimetric nitride using the 4" LPCVD nitride furnace]] | *[[Specific Process Knowledge/Thin film deposition/Furnace LPCVD Nitride/Deposition of stoichiometric nitride using the 4" LPCVD nitride furnace|Deposition of stoichimetric nitride using the 4" LPCVD nitride furnace]] |
Revision as of 10:47, 26 June 2017
Feedback to this page: click here
Deposition of silicon nitride
Deposition of silicon nitride can be done with either LPCVD (Low Pressure Chemical Vapor Deposition) or PECVD (Plasma Enhanced Chemical Vapor Deposition). Stochiometric nitride or silicon rich (low stress) LPCVD nitride is deposited on a batch of wafers in a LPCVD nitride furnace, and PECVD nitride (or oxynitride) is deposited on a few samples at a time in a PECVD system. LPCVD nitride has a good step coverage and a very good uniformity. Using PECVD it is possible to deposit a much lower temperature and a thicker layer of nitride on different types of samples, but the nitride does not cover sidewalls very well.
It is also possible to deposit silicon nitride using the Lesker sputter system.
- Deposition of stoichimetric nitride using the 4" LPCVD nitride furnace
- Deposition of silicon rich (low stress) nitride using the 6" LPCVD nitride furnace
- Nitride deposition using PECVD (or oxynitride)
Comparison of LPCVD, PECVD and Lesker sputter system for silicon nitride deposition
LPCVD | PECVD | Lesker sputter system | |
---|---|---|---|
Generel description | Low Pressure Chemical Vapour Deposition (LPCVD furnace process) | Plasma Enhanced Chemical Vapour Deposition (PECVD process) | Reactive sputtering |
Stoichiometry |
|
Silicon nitride can be doped with boron, phosphorus or germanium |
Unknown |
Film thickness |
Thicker nitride layers can be deposited over more runs (maximum two) |
|
limited by process time.
Deposition rate is ~1.7nm/min |
Process temperature |
|
|
Room temperature (higher temperature possible) |
Step coverage |
|
|
yes, but amount unknown |
Film quality |
|
|
|
KOH etch rate (80 oC) |
|
|
Unknown |
BHF etch rate |
|
|
Unknown |
Batch size |
|
Depending on what PECVD you use |
|
Allowed materials |
Processed wafers have to be RCA cleaned |
|
Any |