'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Characterization/XRD/HighScore_analysis click here]''' | '''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Characterization/XRD/HighScore_analysis click here]''' | ||
<i> This page is written by <b>DTU Nanolab internal</b></i> | |||
=HighScore Plus= | =HighScore Plus= | ||
HighScore Plus is the software package supplied with the Malvern Panalytical Aeris benchtop Powder XRD. This software is available on the shared data analysis computer located in 346-904 just to the right of the XRD Powder. You can log onto this computer either directly when you are sitting in front of it or through remote desktop from your own computer. | HighScore Plus is the software package supplied with the Malvern Panalytical Aeris benchtop Powder XRD. This software is available on the shared data analysis computer located in 346-904 just to the right of the XRD Powder. You can log onto this computer either directly when you are sitting in front of it or through remote desktop from your own computer. For more details on how to login remotely, please see [https://labmanager.dtu.dk/view_binary.php?fileId=5533 this note] in LabManager - requires login. | ||
==Using HighScore Plus== | ==Using HighScore Plus== | ||
For a guide to use this software, we recommend that users try to follow the tutorial found on [ | For a guide to use this software, we recommend that users try to follow the tutorial found on [https://labmanager.dtu.dk/view_binary.php?fileId=4294 LabManager] - requires login. | ||
You can also have a look at the [https://wiki.iodp.tamu.edu/display/LMUG/HighScore+Plus+Quick+Start+Guide user friendly High-score quick start guide] on the wiki of the International Ocean Discovery Program, which has a ship, the JOIDES Resolution, aboard which there seems to be a multiuser lab with an Aeris benchtop XRD just like ours. Their wiki has some nice guides, though very oriented towards geological/clay samples. | |||
HighScore Plus has several analysis functions for which there is no license in SmartLab Studio II, including Structure Solution, Structure Refinement, and Rietveld analysis. The software is only suitable for powder analysis. | HighScore Plus has several analysis functions for which there is no license in SmartLab Studio II, including Structure Solution, Structure Refinement, and Rietveld analysis. The software is only suitable for powder analysis. | ||
Latest revision as of 12:24, 22 January 2024
Feedback to this page: click here
This page is written by DTU Nanolab internal
HighScore Plus
HighScore Plus is the software package supplied with the Malvern Panalytical Aeris benchtop Powder XRD. This software is available on the shared data analysis computer located in 346-904 just to the right of the XRD Powder. You can log onto this computer either directly when you are sitting in front of it or through remote desktop from your own computer. For more details on how to login remotely, please see this note in LabManager - requires login.
Using HighScore Plus
For a guide to use this software, we recommend that users try to follow the tutorial found on LabManager - requires login.
You can also have a look at the user friendly High-score quick start guide on the wiki of the International Ocean Discovery Program, which has a ship, the JOIDES Resolution, aboard which there seems to be a multiuser lab with an Aeris benchtop XRD just like ours. Their wiki has some nice guides, though very oriented towards geological/clay samples.
HighScore Plus has several analysis functions for which there is no license in SmartLab Studio II, including Structure Solution, Structure Refinement, and Rietveld analysis. The software is only suitable for powder analysis.