<?xml version="1.0"?>
<feed xmlns="http://www.w3.org/2005/Atom" xml:lang="en">
	<id>https://labadviser.nanolab.dtu.dk//index.php?action=history&amp;feed=atom&amp;title=File%3AWF_2E03_mar23_2011-120c.jpg</id>
	<title>File:WF 2E03 mar23 2011-120c.jpg - Revision history</title>
	<link rel="self" type="application/atom+xml" href="https://labadviser.nanolab.dtu.dk//index.php?action=history&amp;feed=atom&amp;title=File%3AWF_2E03_mar23_2011-120c.jpg"/>
	<link rel="alternate" type="text/html" href="https://labadviser.nanolab.dtu.dk//index.php?title=File:WF_2E03_mar23_2011-120c.jpg&amp;action=history"/>
	<updated>2026-11-06T14:17:32Z</updated>
	<subtitle>Revision history for this page on the wiki</subtitle>
	<generator>MediaWiki 1.43.3</generator>
	<entry>
		<id>https://labadviser.nanolab.dtu.dk//index.php?title=File:WF_2E03_mar23_2011-120c.jpg&amp;diff=4921&amp;oldid=prev</id>
		<title>Jml: Etching of nanostructures in Si using the ICP metal etcher: Sinano3.31 recipe, Run ID 452(abc), 453(bc) and 454 (c), time 60, 120 and 180 secs, BCl3 5, HBr 15, 2mtorr, 900/75 coil/platen, 50 degs.</title>
		<link rel="alternate" type="text/html" href="https://labadviser.nanolab.dtu.dk//index.php?title=File:WF_2E03_mar23_2011-120c.jpg&amp;diff=4921&amp;oldid=prev"/>
		<updated>2011-04-04T11:42:07Z</updated>

		<summary type="html">&lt;p&gt;Etching of nanostructures in Si using the ICP metal etcher: Sinano3.31 recipe, Run ID 452(abc), 453(bc) and 454 (c), time 60, 120 and 180 secs, BCl3 5, HBr 15, 2mtorr, 900/75 coil/platen, 50 degs.&lt;/p&gt;
&lt;p&gt;&lt;b&gt;New page&lt;/b&gt;&lt;/p&gt;&lt;div&gt;Etching of nanostructures in Si using the ICP metal etcher: Sinano3.31 recipe, Run ID 452(abc), 453(bc) and 454 (c), time 60, 120 and 180 secs, BCl3 5, HBr 15, 2mtorr, 900/75 coil/platen, 50 degs.&lt;/div&gt;</summary>