<?xml version="1.0"?>
<feed xmlns="http://www.w3.org/2005/Atom" xml:lang="en">
	<id>https://labadviser.nanolab.dtu.dk//index.php?action=history&amp;feed=atom&amp;title=File%3ABGE_Glass_etch_Cr50Au400n1_pinholes_02.jpg</id>
	<title>File:BGE Glass etch Cr50Au400n1 pinholes 02.jpg - Revision history</title>
	<link rel="self" type="application/atom+xml" href="https://labadviser.nanolab.dtu.dk//index.php?action=history&amp;feed=atom&amp;title=File%3ABGE_Glass_etch_Cr50Au400n1_pinholes_02.jpg"/>
	<link rel="alternate" type="text/html" href="https://labadviser.nanolab.dtu.dk//index.php?title=File:BGE_Glass_etch_Cr50Au400n1_pinholes_02.jpg&amp;action=history"/>
	<updated>2026-08-21T08:25:27Z</updated>
	<subtitle>Revision history for this page on the wiki</subtitle>
	<generator>MediaWiki 1.43.3</generator>
	<entry>
		<id>https://labadviser.nanolab.dtu.dk//index.php?title=File:BGE_Glass_etch_Cr50Au400n1_pinholes_02.jpg&amp;diff=4479&amp;oldid=prev</id>
		<title>BGE: 15min HF 40% etch of borofloat with 50/400 nm Cr/Au mask made in the Alcatel E-beam evaporator. Resist for masking the Cr/Au etch has been left on and baked at 120 degrees of ½ hour. The image is taken where I found some pinholes.</title>
		<link rel="alternate" type="text/html" href="https://labadviser.nanolab.dtu.dk//index.php?title=File:BGE_Glass_etch_Cr50Au400n1_pinholes_02.jpg&amp;diff=4479&amp;oldid=prev"/>
		<updated>2010-12-03T08:11:08Z</updated>

		<summary type="html">&lt;p&gt;15min HF 40% etch of borofloat with 50/400 nm Cr/Au mask made in the Alcatel E-beam evaporator. Resist for masking the Cr/Au etch has been left on and baked at 120 degrees of ½ hour. The image is taken where I found some pinholes.&lt;/p&gt;
&lt;p&gt;&lt;b&gt;New page&lt;/b&gt;&lt;/p&gt;&lt;div&gt;15min HF 40% etch of borofloat with 50/400 nm Cr/Au mask made in the Alcatel E-beam evaporator. Resist for masking the Cr/Au etch has been left on and baked at 120 degrees of ½ hour. The image is taken where I found some pinholes.&lt;/div&gt;</summary>
		<author><name>BGE</name></author>
	</entry>
</feed>