  • curprev 14:5514:55, 7 February 2008Yg talk contribs 394 bytes +394 New page: ==Dope with boron== The furnace A2 boron predep can be used to predeposit silicon wafers with boron. The silicon wafers are positioned in a siliconcarbide boat just next to wafers of boron...