Nano scale etching of silicon nitride with SF6 plasma
Based on silicon etch recipe made by Henri Jansen.
silicon nitride etch
Parameter
|
Silicon nitride etch, platen only
|
SF6 (sccm)
|
5
|
Pressure (APC %)
|
100
|
Platen power (W)
|
20
|
Temperature (oC)
|
20
|