Specific Process Knowledge/Thin film deposition/Deposition of ZnO
Jump to navigation
Jump to search
Feedback to this page: click here
ZnO can be deposited by Sputtering process and atomic layer deposition (ALD). In the chart below your can compare the different deposition equipment.
Sputtering deposition (Lesker) | Atomic layer deposition (ALD Picosun R200) | |
---|---|---|
General description | Sputter deposition of ZnO | Atomic layer deposition of ZnO |
Pre-clean | RF Ar clean | |
Layer thickness | 10Å to 5000Å* | 0 to 1000 Å |
Deposition rate | Depending on process parameters. | Depending on temperature |
Batch size |
|
|
Allowed materials |
|
|
Comment |
|
* For thicknesses above 200 nm permission is required.