Specific Process Knowledge/Thin film deposition/Furnace LPCVD Nitride
At the moment we have one LPCVD furnace for nitride depositions.
A few words about the furnace
The furnace is a Tempress horisontal furnace. The process is a batch process meaning you can run a batch of 25 wafers at a time. The deposition takes place at temperatures of 800-835 degrees Celsius. The reactive gases are Ammonia and dichlorsilane. The LPCVD nitride has a good step coverage and the film thickness is very uniform over the wafer. We have two standard LPCVD nitride processes: One for depositing stoichiometric nitride (Si3N4) and one for deposition of low stress nitride (SNR).
LPCVD | |
---|---|
Stoichiometry |
SRN: Silicon Rich Nitride |
Film thickness |
|
Process Temperature |
|
Step coverage |
|
Film quality |
|
Batch size |
|
Substrate material allowed |
|
Process Knowledge
Please take a look at the process side for deposition of Silicon Nitride using LPCVD: Deposition of Silicon Nitride using LPCVD