Jump to content

Specific Process Knowledge/Lithography/Strip/plasmaAsher03: Difference between revisions

From LabAdviser
Jehem (talk | contribs)
Created page with "=Plasma Asher 3: Descum= 400px|thumb|Plasma Asher 3: Descum is a low power plasma asher dedicated for descumming on smaller substrates. Product name: Diener Pico Plasma Asher<br> Year of purchase: 2014 The Plasma Asher 3: Descum is dedicated for resist descum, i.e. removal of remains resist traces after development. It has a small chamber, so you can only load a single 100 mm substrate, or a few smaller pieces. In this machine, only Ox..."
 
Jehem (talk | contribs)
Line 19: Line 19:
The user manual, user APV, and contact information can be found in [http://labmanager.dtu.dk/function.php?module=Machine&view=view&mach=423 LabManager] - '''requires login'''
The user manual, user APV, and contact information can be found in [http://labmanager.dtu.dk/function.php?module=Machine&view=view&mach=423 LabManager] - '''requires login'''


===Process Information===
==Process Information==
Detailed information about descum processing on Plasma asher 3: Descum can be found [[Specific Process Knowledge/Lithography/Descum|here]].
Detailed information about descum processing on Plasma asher 3: Descum can be found [[Specific Process Knowledge/Lithography/Descum|here]].
<br clear="all" />
<br clear="all" />

Revision as of 12:21, 12 January 2026

Plasma Asher 3: Descum

Plasma Asher 3: Descum is a low power plasma asher dedicated for descumming on smaller substrates.

Product name: Diener Pico Plasma Asher
Year of purchase: 2014

The Plasma Asher 3: Descum is dedicated for resist descum, i.e. removal of remains resist traces after development. It has a small chamber, so you can only load a single 100 mm substrate, or a few smaller pieces.

In this machine, only Oxygen is used for processing.

Typical process parameters:
Process: Photoresist descumming
Pressure: 0.2-0.8 mbar
Gas: 45 sccm O2
Power: 100 W (100%)
Time: 1 -10 minutes (depending on photoresist type and thickness)

Other materials have not been tested.