The Cleaver: Lattice Axe is designed for cleaving wafers into smaller pieces. The equipment is placed in the left drawer underneath fumehood 5: Special purposes. When operated the the Cleaver: lattice axe should always be placed inside Fume hood 5. | The Cleaver: Lattice Axe is designed for cleaving wafers into smaller pieces. The equipment is placed in the left drawer underneath fumehood 5: Special purposes. When operated the the Cleaver: lattice axe should always be placed inside Fume hood 5. | ||
[[File:LatticeAxe placer prøve.JPG|400px]] | |||
'''Approved Materials''': | '''Approved Materials''': | ||
Revision as of 15:07, 31 March 2020
The Cleaver: Lattice Axe is designed for cleaving wafers into smaller pieces. The equipment is placed in the left drawer underneath fumehood 5: Special purposes. When operated the the Cleaver: lattice axe should always be placed inside Fume hood 5.
Approved Materials:
- Si
- Quartz
- Pyrex (Borofloat 33)
- GaAs
- InP
- Sapphire
The LatticeAxe can cleave samples from 100mm down to 10mm. In some cases it can even be used on 150mm samples please contact wetchemistry group for more information