==Dektak 8 stylus profiler==
to be deleted, info copied to pages with respective tool name


[[image:Dektak8.JPG|275x275px|right|thumb|Dektak8: positioned in cleanroom 4 - glass cage no. 3]]
https://labadviser.nanolab.dtu.dk//index.php?title=Specific_Process_Knowledge/Characterization/Dektak_XTA


Dektak 8 stylus profiler is a product of Veeco Instruments. It is usable for profiling surfaces of samples with structures in the micrometer range. It can measure in a specific point found with help from  high magnification video cameras or it can be programmed to measure several points defined with respect to some deskew points. It can also be used for stress measurements of thin films by measuring the wafer bow.
https://labadviser.nanolab.dtu.dk//index.php?title=Specific_Process_Knowledge/Characterization/Tencor_P17


To get some product information and some tips and tricks from the vendor take a look at Veeco's homepage [http://www.veeco.com/products/details.php?cat=1&sub=6&pid=32]
https://labadviser.nanolab.dtu.dk//index.php?title=Specific_Process_Knowledge/Characterization/Sensofar_S_Neox
<br clear="all" />


===A rough overview of the performance of Dektak 8 stylus profiler===
https://labadviser.nanolab.dtu.dk//index.php?title=Specific_Process_Knowledge/Characterization/Filmetrics


{| border="2" cellspacing="0" cellpadding="10"
https://labadviser.nanolab.dtu.dk//index.php?title=Specific_Process_Knowledge/Characterization/Dektak_3ST
|-
!style="background:silver; color:black;" align="left"|Purpose
|style="background:LightGrey; color:black"|Profiler for measuring micro structures.||style="background:WhiteSmoke; color:black"|
*Single point profiles
*Wafer mapping
*Stress measurements by measuring wafer bow
*Surface roughness on a line scan
|-
!style="background:silver; color:black" align="left"|Performance
|style="background:LightGrey; color:black"|Scan range xy||style="background:WhiteSmoke; color:black"|
Line scan x: 50 µm to 100 mm
|-
|style="background:silver; color:black"|
|style="background:LightGrey; color:black"|Scan range z
|style="background:WhiteSmoke; color:black"|
50 Å to 1 mm
|-
|style="background:silver; color:black"|
|style="background:LightGrey; color:black"|Resolution xy
|style="background:WhiteSmoke; color:black"|
down to 0.067 µm
|-
|style="background:silver; color:black"|
|style="background:LightGrey; color:black"|Resolution z
|style="background:WhiteSmoke; color:black"|
1Å, 10Å, 40Å or 160Å (for ranges 65kÅ, 655 kÅ, 2620 kÅ and 1mm respectively)
|-
|style="background:silver; color:black"|
|style="background:LightGrey; color:black"|Max. scan depth as a function of trench width W
|style="background:WhiteSmoke; color:black"|
1.2(W[µm]-5µm)
|-
|-
!style="background:silver; color:black" align="left"|Hardware settings
|style="background:LightGrey; color:black"|Tip radius
|style="background:WhiteSmoke; color:black"|
*5 µm 45<sup>o</sup> cone
|-
!style="background:silver; color:black" align="left"|Substrates
|style="background:LightGrey; color:black"|Substrate size
|style="background:WhiteSmoke; color:black"|
*up to 8"
|-
|style="background:silver; color:black"|
| style="background:LightGrey; color:black"|Substrate material allowed
|style="background:WhiteSmoke; color:black"|
*In principle all materials
|-
|}


==Tencor stylus profiler==
https://labadviser.nanolab.dtu.dk//index.php?title=Specific_Process_Knowledge/Characterization/Dektak_150
 
[[image:TencorP1.jpg|275x275px|right|thumb|Tencor: positioned in cleanroom 4 - glass cage no. 3]]
 
Tencor P1 stylus profiler is a product of KLA-Tencor Corporation. It is usable for profiling surfaces of samples with structures in the micrometer range. It can measure in a specific point found with help from a high magnification video camera. It can also be used for stress measurements of thin films by measuring the wafer bow.
 
It is a very old system and should be treated with care.
<br clear="all" />
 
===Overview of the performance of Tencor P1 stylus profiler===
 
{| border="2" cellspacing="0" cellpadding="10"
|-
!style="background:silver; color:black;" align="left"|Purpose
|style="background:LightGrey; color:black"|Profiler for measuring micro structures. ||style="background:WhiteSmoke; color:black"|
*Single point profiles
*Stress measurements by measuring wafer bow
*Surface roughness on a line scan
|-
!style="background:silver; color:black" align="left"|Performance
|style="background:LightGrey; color:black"|Scan range xy||style="background:WhiteSmoke; color:black"|
Line scan x: Full substrate size
|-
|style="background:silver; color:black"|
|style="background:LightGrey; color:black"|Scan range z
|style="background:WhiteSmoke; color:black"|
<100 Å to ~0.3 mm
|-
|style="background:silver; color:black"|
|style="background:LightGrey; color:black"|Resolution xy
|style="background:WhiteSmoke; color:black"|
up to 5900 data points per profile
|-
|style="background:silver; color:black"|
|style="background:LightGrey; color:black"|Resolution z
|style="background:WhiteSmoke; color:black"|
1Å or 25Å
|-
|style="background:silver; color:black"|
|style="background:LightGrey; color:black"|Max. scan depth as a function of trench width W
|style="background:WhiteSmoke; color:black"|
0.87(W[µm]-5µm)
|-
|-
!style="background:silver; color:black" align="left"|Hardware settings
|style="background:LightGrey; color:black"|Tip radius
|style="background:WhiteSmoke; color:black"|
*5 µm 60<sup>o</sup> cone
|-
!style="background:silver; color:black" align="left"|Substrates
|style="background:LightGrey; color:black"|Substrate size
|style="background:WhiteSmoke; color:black"|
*up to 4"
|-
|style="background:silver; color:black"|
| style="background:LightGrey; color:black"|Substrate material allowed
|style="background:WhiteSmoke; color:black"|
*In principle all materials
|-
|}
 
==Comparing the profilers==
Take a look at the [[Specific Process Knowledge/Characterization/Topographic measurement|topographic measurement]] page.

Latest revision as of 21:52, 27 May 2025