Specific Process Knowledge/Back-end processing/Polishing machine: Difference between revisions
Jump to navigation
Jump to search
No edit summary |
|||
Line 5: | Line 5: | ||
[[image:Logitech pm5 1.jpg|400px|right|thumb|The Logitech PM5 Polisher/Lapper]] | [[image:Logitech pm5 1.jpg|400px|right|thumb|The Logitech PM5 Polisher/Lapper]] | ||
Training is required before using th machine. The machine is equipped with a LabManager lock. | |||
The Logitech PM5 Polisher/Lapper is for thinning down wafers and other substrates. | The Logitech PM5 Polisher/Lapper is for thinning down wafers and other substrates. |
Revision as of 10:26, 21 September 2022
Feedback to this page: click here
Polisher/Lapper
Training is required before using th machine. The machine is equipped with a LabManager lock.
The Logitech PM5 Polisher/Lapper is for thinning down wafers and other substrates.
The user manual, user APV, technical information and contact information can be found in LabManager:
The Logitech PM5 Polisher/Lapper in LabManager
Equipment | Polisher/Lapper | |
---|---|---|
Purpose |
Thinning of substrates of |
|
Performance | Thinning |
|
Polishing |
| |
Process parameter range | Polishing liquid |
|
Polishing cloths |
| |
Rotation speed |
| |
Arm sweep |
| |
Substrates | Batch size |
|
Allowed materials |
|